General
Property | Value | Comment |
---|---|---|
Density | 8.62 g/cm³ Show Material materials with Density of 8.62 g/cm³ | Predicted Value |
Grain size | 0.031 μm Show Material materials with Grain size of 0.031 μm | Predicted Value |
Mechanical
Property | Value | Related Standards | Shape | Comment |
---|---|---|---|---|
Compressive strength | 1215 MPa Show Material materials with Compressive strength of 1215 MPa | Predicted Value | ||
Elastic modulus | 96 - 120 GPa Show Material materials with Elastic modulus of 96 - 120 GPa | Typical for Cast Copper Bronze | ||
Fatigue strength | 395 MPa Show Material materials with Fatigue strength of 395 MPa | Predicted Value | ||
Hardness, Brinell | 110 [-] Show Material materials with Hardness, Brinell of 110 [-] | Predicted Value | ||
Hardness, HBW | 249.8 [-] Show Material materials with Hardness, HBW of 249.8 [-] | Predicted Value | ||
Hardness, Rockwell F | 80 [-] Show Material materials with Hardness, Rockwell F of 80 [-] | Predicted Value | ||
Hardness, Rockwell Superficial 15-N | 73 [-] Show Material materials with Hardness, Rockwell Superficial 15-N of 73 [-] | Predicted Value | ||
Hardness, Rockwell Superficial 30-N | 45 [-] Show Material materials with Hardness, Rockwell Superficial 30-N of 45 [-] | Predicted Value | ||
Hardness, Rockwell Superficial 30-T | 55 [-] Show Material materials with Hardness, Rockwell Superficial 30-T of 55 [-] | Predicted Value | ||
Hardness, Vickers | 129 [-] Show Material materials with Hardness, Vickers of 129 [-] | Predicted Value | ||
Poisson's ratio | 0.34 [-] Show Material materials with Poisson's ratio of 0.34 [-] | Typical for Cast Copper Bronze | ||
Reduction of area | 58.4 % Show Material materials with Reduction of area of 58.4 % | Predicted Value | ||
Shear modulus | 45.0 GPa Show Material materials with Shear modulus of 45.0 GPa | Predicted Value | ||
Shear strength | 236.7 MPa Show Material materials with Shear strength of 236.7 MPa | Predicted Value | ||
Tensile strength | 276 MPa Show Material materials with Tensile strength of 276 MPa | ASTM B505 | Casting |
Thermal
Property | Value | Comment |
---|---|---|
Coefficient of thermal expansion | 1.6e-05 - 1.9e-05 1/K Show Material materials with Coefficient of thermal expansion of 1.6e-05 - 1.9e-05 1/K | Typical for Cast Copper Bronze |
Melting point | 760 - 1060 °C Show Material materials with Melting point of 760 - 1060 °C | Typical for Cast Copper Bronze |
Specific heat capacity | 376 - 440 J/(kg·K) Show Material materials with Specific heat capacity of 376 - 440 J/(kg·K) | Typical for Cast Copper Bronze |
Thermal conductivity | 12 - 81 W/(m·K) Show Material materials with Thermal conductivity of 12 - 81 W/(m·K) | Typical for Cast Copper Bronze |
Electrical
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Aluminium | 0.005 % Show Material materials with Aluminium of 0.005 % | ASTM B505 | Casting |
Antimony | 0.2 % Show Material materials with Antimony of 0.2 % | ASTM B505 | Casting |
Copper | 88 - 90 % Show Material materials with Copper of 88 - 90 % | ASTM B505 | Casting |
Iron | 0.15 % Show Material materials with Iron of 0.15 % | ASTM B505 | Casting |
Lead | 0.5 % Show Material materials with Lead of 0.5 % | ASTM B505 | Casting |
Nickel | 0.5 % Show Material materials with Nickel of 0.5 % | ASTM B505 | Casting |
Phosphorus | 1.5 % Show Material materials with Phosphorus of 1.5 % | ASTM B505 | Casting |
Silicon | 0.005 % Show Material materials with Silicon of 0.005 % | ASTM B505 | Casting |
Sulfur | 0.05 % Show Material materials with Sulfur of 0.05 % | ASTM B505 | Casting |
Tin | 10 - 12 % Show Material materials with Tin of 10 - 12 % | ASTM B505 | Casting |
Zinc | 0.5 % Show Material materials with Zinc of 0.5 % | ASTM B505 | Casting |