Yield strength Rp0.05: 900 MPa

Quick Comparison

Wrought Copper Nickel Grade

ASTM B740 Grade C72900 TM08

Wrought Copper Nickel Grade

ASTM B740 Grade C72650 TS04

Wrought Copper Nickel Grade

ASTM B740 Grade C72700 TS04

Wrought Copper Nickel Grade

ASTM B740 Grade C72700 TS08

Wrought Copper Nickel Grade

ASTM B740 Grade C72700 TS12

Wrought Copper Nickel Grade

ASTM B740 Grade C72900 TS02