General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 8.95 g/cm³ Show Material materials with Density of 8.95 g/cm³ | Typical for Wrought Copper Nickel Grade |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 120 - 156 GPa Show Material materials with Elastic modulus of 120 - 156 GPa | Typical for Wrought Copper Nickel Grade |
Elongation A50 | 23.0 °C | 2 % Show Material materials with Elongation A50 of 2 % | |
Tensile strength | 23.0 °C | 1035 - 1225 MPa Show Material materials with Tensile strength of 1035 - 1225 MPa | |
Yield strength Rp0.05 | 23.0 °C | 860 - 1035 MPa Show Material materials with Yield strength Rp0.05 of 860 - 1035 MPa | |
Yield strength Rp0.2 | 23.0 °C | 140 - 170 MPa Show Material materials with Yield strength Rp0.2 of 140 - 170 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.4E-5 - 1.8E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.4E-5 - 1.8E-5 1/K | Typical for Wrought Copper Nickel Grade |
Melting point | 915 - 1240 °C Show Material materials with Melting point of 915 - 1240 °C | Typical for Wrought Copper Nickel Grade | |
Specific heat capacity | 23.0 °C | 375 - 398 J/(kg·K) Show Material materials with Specific heat capacity of 375 - 398 J/(kg·K) | Typical for Wrought Copper Nickel Grade |
Thermal conductivity | 23.0 °C | 21 - 195 W/(m·K) Show Material materials with Thermal conductivity of 21 - 195 W/(m·K) | Typical for Wrought Copper Nickel Grade |
Chemical properties
Property | Value |
---|---|
Iron | 0.5 % Show Material materials with Iron of 0.5 % |
Lead | 0.02 % Show Material materials with Lead of 0.02 % |
Magnesium | 0.15 % Show Material materials with Magnesium of 0.15 % |
Manganese | 0.3 % Show Material materials with Manganese of 0.3 % |
Nickel | 14.5 - 15.5 % Show Material materials with Nickel of 14.5 - 15.5 % |
Niobium | 0.1 % Show Material materials with Niobium of 0.1 % |
Tin | 7.5 - 8.5 % Show Material materials with Tin of 7.5 - 8.5 % |
Zinc | 0.5 % Show Material materials with Zinc of 0.5 % |