Límite elástico Rp0.5: 724 MPa

Quick Comparison

Cast Copper Bronze Aluminium Bronze

AMPCO® M4 Centrifugal castings

Suministrada por:

AMPCO METAL

Wrought Copper Bronze Aluminium Bronze

AMPCO® M4 Extrusions

Suministrada por:

AMPCO METAL

Cast Copper Bronze Aluminium Bronze

AMPCO® M4 Sand castings

Suministrada por:

AMPCO METAL

Cast Copper Nickel Grade

ASTM B505 Grade C96900 Heat-Treated