Acero inoxidable austenítico
EN 10272 Grade X2CrNi18-9 solution annealed (+AT)Acero inoxidable austenítico
EN 10028-7 Grade X5NiCrAlTi31-20 solution annealed (+AT)Acero inoxidable austenítico
EN 10216-5 Grade X1CrNi25-21 solution annealed (+AT)Acero inoxidable austenítico
EN 10216-5 Grade X2NiCrAlTi32-20 solution annealed (+AT)Acero inoxidable austenítico
SEW 400 Grade X1CrNi25-21 quenched (+Q)Acero inoxidable austenítico
EN 10250-4 Grade X2CrNi18-9 solution annealed (+AT)Nickel Chromium Molybdenum Alloy
DIN 17744 Grade NiMo16Cr15W solution heat-treated and quenched