Acero inoxidable austenítico
DIN 17440 Grade X6CrNiTi18-10 solution heat-treated and quenchedAcero inoxidable austenítico
EN 10272 Grade X2CrNi18-9 solution annealed (+AT)Aleación casi alfa
VdTÜV WB 230-3 Grade TiNi0.8Mo0.3 AnnealedSuministrada por:
2 proveedores de Matmatch
Acero inoxidable austenítico
EN 10216-5 Grade X6CrNiTi18-10 solution annealed (+AT)Acero inoxidable austenítico
EN 10216-5 Grade X6CrNiMoTi17-12-2 solution annealed (+AT)Acero inoxidable austenítico
EN 10028-7 Grade X6CrNi23-13 solution annealed (+AT)Acero inoxidable austenítico
EN 10028-7 Grade X6CrNi25-20 solution annealed (+AT)Acero inoxidable austenítico
EN 10217-7 Grade X6CrNiMoTi17-12-2 solution annealed (+AT)Acero inoxidable austenítico
EN 10217-7 Grade X6CrNiTi18-10 solution annealed (+AT)Wrought Copper Nickel Grade
EN 1652 Grade CuNi10Fe1Mn R300Wrought Copper Nickel Grade
EN 1652 Grade CuNi30Mn1Fe H080Wrought Copper Nickel Grade
EN 12163 Grade CuNi30Mn1Fe R340Wrought Copper Nickel Grade
EN 12451 Grade CuNi30Mn1Fe R370Wrought Copper Nickel Grade
EN 12451 Grade CuNi30Mn1Fe H090Wrought Copper Nickel Grade
EN 12452 Grade CuNi30Mn1Fe R370