VdTÜV WB 230-3 Grade TiNi0.8Mo0.3 Annealed

Want to keep this datasheet? Save it now in your required format

Description

This DIN TiNi0.8Mo0.3 alloy is similar to Titanium Grades 2 and 3 except that DIN TiNi0.8Mo0.3 has 0.3% molybdenum and 0.8% nickel. This alloy also offers enhanced corrosion resistance.

Related Standards

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueConditionRelated StandardsShape

Density

20.0 °C

4.505 g/cm³

Show Material materials with Density of 4.505 g/cm³

Annealed

VdTÜV WB 230-3, DIN 17851, DIN 17862, DIN 17864, DIN 17860, DIN 17850, VdTÜV WB 230-1, VdTÜV WB 230-2

Forging, Rod, Wire, Bar, Tube, Flat

20.0 °C

4.51 g/cm³

Show Material materials with Density of 4.51 g/cm³

Annealed

DIN 17851, VdTÜV WB 230-2, DIN 17862, DIN 17864, DIN 17860, VdTÜV WB 230-1, VdTÜV WB 230-3

Forging, Rod, Welded Tube

Mechanical

PropertyTemperatureValueConditionRelated StandardsShapeComment

Elastic modulus

20.0 °C

103.0 GPa

Show Material materials with Elastic modulus of 103.0 GPa

Annealed

DIN 17851, DIN 17864, DIN 17862, DIN 17860, VdTÜV WB 230-1, VdTÜV WB 230-2, VdTÜV WB 230-3

Forging, Rod, Welded Tube

20.0 °C

108.0 - 110.0 GPa

Show Material materials with Elastic modulus of 108.0 - 110.0 GPa

Annealed

DIN 17851, VdTÜV WB 230-3, DIN 17862, DIN 17864, DIN 17860, DIN 17850, VdTÜV WB 230-1, VdTÜV WB 230-2

Forging, Rod, Tube, Flat, Wire, Bar

200.0 °C

96.0 - 97.0 GPa

Show Material materials with Elastic modulus of 96.0 - 97.0 GPa

Annealed

DIN 17851, VdTÜV WB 230-3, DIN 17862, DIN 17864, DIN 17860, DIN 17850, VdTÜV WB 230-1, VdTÜV WB 230-2

Forging, Rod, Tube, Flat, Wire, Bar

400.0 °C

82.0 GPa

Show Material materials with Elastic modulus of 82.0 GPa

Annealed

DIN 17851, VdTÜV WB 230-3, DIN 17862, DIN 17864, DIN 17860, DIN 17850, VdTÜV WB 230-1, VdTÜV WB 230-2

Forging, Rod, Tube, Flat, Wire, Bar

Elongation

20.0 °C

16.0 %

Show Material materials with Elongation of 16.0 %

Annealed

DIN 17850, VdTÜV WB 230-3, DIN 17851, DIN 17862, DIN 17864, DIN 17860, VdTÜV WB 230-1, VdTÜV WB 230-2

Forging, Rod

Transverse

20.0 °C

18.0 %

Show Material materials with Elongation of 18.0 %

Annealed

DIN 17850, VdTÜV WB 230-3, DIN 17851, DIN 17862, DIN 17864, DIN 17860, VdTÜV WB 230-1, VdTÜV WB 230-2

Forging, Rod, Welded Tube

Hardness, Brinell

20.0 °C

170.0

Show Material materials with Hardness, Brinell of 170.0

Annealed

DIN 17850, VdTÜV WB 230-3, DIN 17851, DIN 17862, DIN 17864, DIN 17860, VdTÜV WB 230-1, VdTÜV WB 230-2

Forging, Rod

20.0 °C

170.0

Show Material materials with Hardness, Brinell of 170.0

Annealed

DIN 17864, DIN 17851, DIN 17862, DIN 17860

Forging

Transverse

Reduction of area

20.0 °C

25.0 %

Show Material materials with Reduction of area of 25.0 %

Annealed

DIN 17850, VdTÜV WB 230-3, DIN 17851, DIN 17862, DIN 17864, DIN 17860, VdTÜV WB 230-1, VdTÜV WB 230-2

Forging, Rod

Tensile strength

20.0 °C

480.0 MPa

Show Material materials with Tensile strength of 480.0 MPa

Annealed

DIN 17850, VdTÜV WB 230-3, DIN 17851, DIN 17862, DIN 17864, DIN 17860, VdTÜV WB 230-1, VdTÜV WB 230-2

Forging, Rod, Welded Tube

20.0 °C

480.0 MPa

Show Material materials with Tensile strength of 480.0 MPa

Annealed

DIN 17850, VdTÜV WB 230-3, DIN 17851, DIN 17862, DIN 17864, DIN 17860, VdTÜV WB 230-1, VdTÜV WB 230-2

Forging, Rod

Transverse

20.0 °C

560.0 MPa

Show Material materials with Tensile strength of 560.0 MPa

Annealed

DIN 17850, VdTÜV WB 230-3, DIN 17851, DIN 17862, DIN 17864, DIN 17860, VdTÜV WB 230-1, VdTÜV WB 230-2

100.0 °C

460.0 MPa

Show Material materials with Tensile strength of 460.0 MPa

Annealed

DIN 17850, VdTÜV WB 230-3, DIN 17851, DIN 17862, DIN 17864, DIN 17860, VdTÜV WB 230-1, VdTÜV WB 230-2

200.0 °C

340.0 MPa

Show Material materials with Tensile strength of 340.0 MPa

Annealed

DIN 17850, VdTÜV WB 230-3, DIN 17851, DIN 17862, DIN 17864, DIN 17860, VdTÜV WB 230-1, VdTÜV WB 230-2

300.0 °C

260.0 MPa

Show Material materials with Tensile strength of 260.0 MPa

Annealed

DIN 17850, VdTÜV WB 230-3, DIN 17851, DIN 17862, DIN 17864, DIN 17860, VdTÜV WB 230-1, VdTÜV WB 230-2

Thermal

PropertyTemperatureValueConditionRelated StandardsShapeComment

Coefficient of thermal expansion

7.599999999999997e-06 - 1.1e-05 1/K

Show Material materials with Coefficient of thermal expansion of 7.599999999999997e-06 - 1.1e-05 1/K

Typical for Titanium Near Alpha Alloy

Melting point

1540.0 - 1715.0 °C

Show Material materials with Melting point of 1540.0 - 1715.0 °C

Typical for Titanium Near Alpha Alloy

Specific heat capacity

20.0 °C

520.0 J/(kg·K)

Show Material materials with Specific heat capacity of 520.0 J/(kg·K)

Annealed

VdTÜV WB 230-3, DIN 17851, DIN 17862, DIN 17864, DIN 17860, DIN 17850, VdTÜV WB 230-1, VdTÜV WB 230-2

Forging, Rod, Wire, Bar, Tube, Flat

200.0 °C

570.0 J/(kg·K)

Show Material materials with Specific heat capacity of 570.0 J/(kg·K)

Annealed

VdTÜV WB 230-3, DIN 17851, DIN 17862, DIN 17864, DIN 17860, DIN 17850, VdTÜV WB 230-1, VdTÜV WB 230-2

Forging, Rod, Wire, Bar, Tube, Flat

400.0 °C

630.0 J/(kg·K)

Show Material materials with Specific heat capacity of 630.0 J/(kg·K)

Annealed

VdTÜV WB 230-3, DIN 17851, DIN 17862, DIN 17864, DIN 17860, DIN 17850, VdTÜV WB 230-1, VdTÜV WB 230-2

Forging, Rod, Wire, Bar, Tube, Flat

Thermal conductivity

20.0 °C

19.0 W/(m·K)

Show Material materials with Thermal conductivity of 19.0 W/(m·K)

Annealed

DIN 17851, DIN 17864, DIN 17862, DIN 17860, VdTÜV WB 230-1, VdTÜV WB 230-2, VdTÜV WB 230-3

Forging, Rod, Welded Tube

20.0 °C

22.6 W/(m·K)

Show Material materials with Thermal conductivity of 22.6 W/(m·K)

Annealed

DIN 17851, VdTÜV WB 230-3, DIN 17862, DIN 17864, DIN 17860, DIN 17850, VdTÜV WB 230-1, VdTÜV WB 230-2

Forging, Rod, Tube, Flat, Wire, Bar

200.0 °C

20.9 W/(m·K)

Show Material materials with Thermal conductivity of 20.9 W/(m·K)

Annealed

DIN 17851, VdTÜV WB 230-3, DIN 17862, DIN 17864, DIN 17860, DIN 17850, VdTÜV WB 230-1, VdTÜV WB 230-2

Forging, Rod, Tube, Flat, Wire, Bar

400.0 °C

19.3 W/(m·K)

Show Material materials with Thermal conductivity of 19.3 W/(m·K)

Annealed

DIN 17851, VdTÜV WB 230-3, DIN 17862, DIN 17864, DIN 17860, DIN 17850, VdTÜV WB 230-1, VdTÜV WB 230-2

Forging, Rod, Tube, Flat, Wire, Bar

Electrical

PropertyTemperatureValueConditionRelated StandardsShape

Electrical resistivity

20.0 °C

5.2e-07 Ω·m

Show Material materials with Electrical resistivity of 5.2e-07 Ω·m

Annealed

DIN 17851, DIN 17864, DIN 17862, DIN 17860, VdTÜV WB 230-1, VdTÜV WB 230-2, VdTÜV WB 230-3, DIN 17850

Forging, Rod, Welded Tube, Tube, Flat, Wire, Bar

200.0 °C

8.7e-07 Ω·m

Show Material materials with Electrical resistivity of 8.7e-07 Ω·m

Annealed

DIN 17851, VdTÜV WB 230-3, DIN 17862, DIN 17864, DIN 17860, DIN 17850, VdTÜV WB 230-1, VdTÜV WB 230-2

Forging, Rod, Tube, Flat, Wire, Bar

400.0 °C

1.2e-06 Ω·m

Show Material materials with Electrical resistivity of 1.2e-06 Ω·m

Annealed

DIN 17851, VdTÜV WB 230-3, DIN 17862, DIN 17864, DIN 17860, DIN 17850, VdTÜV WB 230-1, VdTÜV WB 230-2

Forging, Rod, Tube, Flat, Wire, Bar

Chemical properties

PropertyValueConditionRelated StandardsShape

Carbon

0.06

Show Material materials with Carbon of 0.06

Annealed

VdTÜV WB 230-3, DIN 17851, DIN 17862, DIN 17864, DIN 17860, DIN 17850, VdTÜV WB 230-1, VdTÜV WB 230-2

Forging, Rod, Wire, Bar, Tube, Welded Tube, Flat

Hydrogen

0.013

Show Material materials with Hydrogen of 0.013

Annealed

VdTÜV WB 230-3, DIN 17851, DIN 17862, DIN 17864, DIN 17860, DIN 17850, VdTÜV WB 230-1, VdTÜV WB 230-2

Forging, Rod, Wire, Bar, Tube, Welded Tube, Flat

Iron

0.25

Show Material materials with Iron of 0.25

Annealed

VdTÜV WB 230-3, DIN 17851, DIN 17862, DIN 17864, DIN 17860, DIN 17850, VdTÜV WB 230-1, VdTÜV WB 230-2

Forging, Rod, Wire, Bar, Tube, Welded Tube, Flat

Molybdenum

0.2 - 0.4 %

Show Material materials with Molybdenum of 0.2 - 0.4 %

Annealed

VdTÜV WB 230-3, DIN 17851, DIN 17862, DIN 17864, DIN 17860, DIN 17850, VdTÜV WB 230-1, VdTÜV WB 230-2

Forging, Rod, Wire, Bar, Tube, Welded Tube, Flat

Nickel

0.6 - 0.9 %

Show Material materials with Nickel of 0.6 - 0.9 %

Annealed

VdTÜV WB 230-3, DIN 17851, DIN 17862, DIN 17864, DIN 17860, DIN 17850, VdTÜV WB 230-1, VdTÜV WB 230-2

Forging, Rod, Wire, Bar, Tube, Welded Tube, Flat

Nitrogen

0.03

Show Material materials with Nitrogen of 0.03

Annealed

VdTÜV WB 230-3, DIN 17851, DIN 17862, DIN 17864, DIN 17860, DIN 17850, VdTÜV WB 230-1, VdTÜV WB 230-2

Forging, Rod, Wire, Bar, Tube, Welded Tube, Flat

Oxygen

0.25

Show Material materials with Oxygen of 0.25

Annealed

VdTÜV WB 230-3, DIN 17851, DIN 17862, DIN 17864, DIN 17860, DIN 17850, VdTÜV WB 230-1, VdTÜV WB 230-2

Forging, Rod, Wire, Bar, Tube, Welded Tube, Flat

Titanium

97.7 %

Show Material materials with Titanium of 97.7 %

Annealed

DIN 17851, VdTÜV WB 230-2, DIN 17862, DIN 17864, DIN 17860, VdTÜV WB 230-1, VdTÜV WB 230-3

Tube, Forging, Rod, Welded Tube