7000 Serie
AA Standards Grade 7034Cast Copper Silicon Brass
ASTM B176 Grade C87800Cast Copper Silicon Brass
ASTM B176 Grade C87800Cast Copper Silicon Brass
ASTM B584 Grade C87400Cast Copper Silicon Brass
ASTM B584 Grade C87500Red Brass
ASTM B505 Grade C84200Cast Copper Silicon Brass
ASTM B271 Grade C87400 As-CastCast Copper Silicon Brass
ASTM B271 Grade C87500 As-CastRed Brass
ASTM B505 Grade C84200Cast Copper Silicon Brass
ASTM B584 Grade C87400Cast Copper Silicon Brass
ASTM B584 Grade C87500Cast Copper Silicon Brass
ASTM B763 Grade C87400 Separately Cast Test BarsCast Copper Silicon Brass
ASTM B763 Grade C87500 Separately Cast Test BarsCast Copper Silicon Brass
AS/NZS 1565 Grade C87800Red Brass
JIS H5101 Grade YBsC 1Other Copper Zinc Alloy
ASTM B694 Grade C66400 O60Other Copper Zinc Alloy
ASTM B694 Grade C66410 O60Cast Copper Bronze
JIS H5111 Grade BC 1Cast Copper Bronze
JIS H2203 Grade BC In 1