General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 8.47 g/cm³ Show Material materials with Density of 8.47 g/cm³ | Typical for Cast Copper Brass Yellow Brass |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Charpy impact energy | 23.0 °C | 95 J Show Material materials with Charpy impact energy of 95 J | |
Elastic modulus | 23.0 °C | 108 GPa Show Material materials with Elastic modulus of 108 GPa | |
Elongation A50 | 23.0 °C | 25 % Show Material materials with Elongation A50 of 25 % | |
Hardness, Rockwell B | 23.0 °C | 85 - 90 [-] Show Material materials with Hardness, Rockwell B of 85 - 90 [-] | |
Poisson's ratio | 23.0 °C | 0.34 [-] Show Material materials with Poisson's ratio of 0.34 [-] | Typical for Cast Copper Brass Yellow Brass |
Tensile strength | 23.0 °C | 379 MPa Show Material materials with Tensile strength of 379 MPa | |
Yield strength Rp0.2 | 23.0 °C | 207 MPa Show Material materials with Yield strength Rp0.2 of 207 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.5E-5 - 1.9E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.5E-5 - 1.9E-5 1/K | Typical for Cast Copper Brass Yellow Brass |
Melting point | 905 - 932 °C Show Material materials with Melting point of 905 - 932 °C | Typical for Cast Copper Brass Yellow Brass | |
Specific heat capacity | 23.0 °C | 335 - 390 J/(kg·K) Show Material materials with Specific heat capacity of 335 - 390 J/(kg·K) | Typical for Cast Copper Brass Yellow Brass |
Thermal conductivity | 23.0 °C | 116 W/(m·K) Show Material materials with Thermal conductivity of 116 W/(m·K) | Typical for Cast Copper Brass Yellow Brass |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.15 % Show Material materials with Aluminium of 0.15 % |
Antimony | 0.05 % Show Material materials with Antimony of 0.05 % |
Arsenic | 0.05 % Show Material materials with Arsenic of 0.05 % |
Copper | 80 % Show Material materials with Copper of 80 % |
Iron | 0.15 % Show Material materials with Iron of 0.15 % |
Lead | 0.09 % Show Material materials with Lead of 0.09 % |
Magnesium | 0.01 % Show Material materials with Magnesium of 0.01 % |
Manganese | 0.15 % Show Material materials with Manganese of 0.15 % |
Nickel | 0.2 % Show Material materials with Nickel of 0.2 % |
Phosphorus | 0.01 % Show Material materials with Phosphorus of 0.01 % |
Silicon | 3.8 - 4.2 % Show Material materials with Silicon of 3.8 - 4.2 % |
Sulfur | 0.05 % Show Material materials with Sulfur of 0.05 % |
Tin | 0.25 % Show Material materials with Tin of 0.25 % |
Zinc | 12 - 16 % Show Material materials with Zinc of 12 - 16 % |