Zinc: 13.7 %

Quick Comparison

Cast Copper Silicon Brass

ASTM B176 Grade C87800

Cast Copper Silicon Brass

ASTM B176 Grade C87800

Wrought Copper Brass Yellow Brass

CuZn15 Hard

Suministrada por:

Salomon's Metalen

Wrought Copper Brass Yellow Brass

CuZn15 Soft

Suministrada por:

Salomon's Metalen

Cast Copper Silicon Brass

ASTM B584 Grade C87400

Cast Copper Silicon Brass

ASTM B584 Grade C87500

Cast Copper Silicon Brass

ASTM B271 Grade C87400 As-Cast

Cast Copper Silicon Brass

ASTM B271 Grade C87500 As-Cast

Cast Copper Silicon Brass

ASTM B584 Grade C87400

Cast Copper Silicon Brass

ASTM B584 Grade C87500

Wrought Copper Brass Yellow Brass

UNS C23000 H02
Página 1 de 2