Acero de alto carbono
DIN 17200 Grade C60 normalized or normalized formed (+N)Acero de alto carbono
EN 10250-2 Grade C60 normalized and tempered (+NT)Acero de alto carbono
EN 10277-5 Grade C60 cold drawn or turned and quenched and temperedAcero de alto carbono
EN 10083-2 Grade C60 quenched and tempered (+QT)Acero de alto carbono
EN 10083-2 Grade C60 quenched and tempered (+QT)Acero de alto carbono
DIN 17222 Grade C60 cold rolled and hardenedAcero de alto carbono
EN 10277-5 Grade C60 cold drawnAcero de alto carbono
EN 10277-5 Grade C60 cold drawn or turned and normalizedAcero de alto carbono
EN 10083-2 Grade C60 normalized or normalized formed (+N)Acero de alto carbono
EN 10277-2 Grade C60 cold drawnAcero de alto carbono
EN 10083-2 Grade C60 normalized or normalized formed (+N)Acero de alto carbono
EN 10297-1 Grade C60 quenched and tempered (+QT)Acero de alto carbono
EN 10277-2 Grade C60 as rolled and turned (+SH)Acero de alto carbono
EN 10297-1 Grade C60 normalized or normalized formed (+N)Acero de alto carbono
EN 10277-5 Grade C60 cold drawn or turned and soft annealedAcero de alto carbono
DIN 17200 Grade C60 treated for cold shearing (+S)Acero de alto carbono
AISI 1060 Annealed And Cold DrawnAcero de alto carbono
AISI 1060 Hot RolledAcero de alto carbono
AISI 1060 Spheroidized And Cold DrawnAcero de alto carbono
JIS G4802 Grade S60C annealed