DIN 1.4466

Quick Comparison

Acero inoxidable austenítico

Sandvik 2RE69

Suministrada por:

Alleima (formerly Sandvik Materials Technology)

Acero inoxidable austenítico

ASTM A240 Grade 310MoLN Heat-Treated

Acero inoxidable austenítico

ASTM A182 Grade F310MoLN Solution-Annealed

Acero inoxidable austenítico

SAE J405 Grade 310MoLN