Acero inoxidable martensítico
DIN 17240 Grade X19CrMoVNbN11-1 quenched and tempered (+QT)Acero inoxidable martensítico
EN 10269 Grade X19CrMoNbVN11-1 quenched and tempered (+QT)Acero inoxidable martensítico
EN 10269 Grade X19CrMoNbVN11-1 soft annealed (+A)Acero inoxidable martensítico
JIS G4311 Grade SUH600 quenched and temperedAcero inoxidable martensítico
JIS G4311 Grade SUH600 annealed