Chromium Molybdenum Steel
DIN 17176 Grade 12CrMo19-5 soft annealed (+A)Chromium Molybdenum Steel
DIN 17176 Grade 12CrMo19-5 quenched and tempered (+QT2)Chromium Molybdenum Steel
DIN 17176 Grade 12CrMo19-5 quenched and tempered (+QT1)Chromium Molybdenum Steel
EN 10222-2 Grade X16CrMo5-1 normalized and tempered or quenched and temperedChromium Molybdenum Steel
EN 10222-2 Grade X16CrMo5-1 soft annealed (+A)Chromium Molybdenum Steel
ASTM A193 Grade B5 Up to M100, inclChromium Molybdenum Steel
JIS G3458 Grade STPA25Chromium Molybdenum Steel
JIS G3462 Grade STBA25Chromium Molybdenum Steel
JIS G3467 Grade STFA25Chromium Molybdenum Steel
ASTM A335 Grade P5 Heat-TreatedChromium Molybdenum Steel
JIS G3203 Grade SFVAF5BChromium Molybdenum Steel
JIS G3203 Grade SFVAF5CChromium Molybdenum Steel
JIS G3203 Grade SFVAF5DChromium Molybdenum Steel
JIS G4107 Grade SNB5Chromium Molybdenum Steel
JIS G4109 Grade SCMV6Chromium Molybdenum Steel
ASTM A213 Grade T5