Medium Carbon Steel
DIN 17200 Grade C35 normalized or normalized formed (+N)Medium Carbon Steel
EN 10250-2 Grade C35 normalized and tempered (+NT)Medium Carbon Steel
EN 10277-5 Grade C35 cold drawn or turned and quenched and temperedMedium Carbon Steel
DIN 17200 Grade C35 quenched and tempered (+QT)Medium Carbon Steel
EN 10083-2 Grade C35 quenched and tempered (+QT)Medium Carbon Steel
EN 10083-2 Grade C35 quenched and tempered (+QT)Medium Carbon Steel
EN 10277-5 Grade C35 cold drawnMedium Carbon Steel
EN 10277-5 Grade C35 cold drawn or turned and normalizedMedium Carbon Steel
EN 10277-2 Grade C35 cold drawnMedium Carbon Steel
EN 10297-1 Grade C35 quenched and tempered (+QT)Medium Carbon Steel
EN 10277-2 Grade C35 as rolled and turned (+SH)Medium Carbon Steel
EN 10297-1 Grade C35 normalized or normalized formed (+N)Medium Carbon Steel
EN 10083-2 Grade C35 soft annealed (+A)Medium Carbon Steel
JIS G4051 Grade S35CMedium Carbon Steel
SAE J118 Grade 1034