DIN 1.6523

Quick Comparison

Nickel Chromium Molybdenum Steel

DIN 1652-3 Grade 21NiCrMo2 cold drawn

Nickel Chromium Molybdenum Steel

EN 10084 Grade 20NiCrMo2-2 quenched (+Q)

Nickel Chromium Molybdenum Steel

DIN 17210 Grade 21NiCrMo2 soft annealed (+A)

Chromium Molybdenum Steel

AISI 8620 Annealed

Chromium Molybdenum Steel

AISI 8620 Normalized

Nickel Chromium Molybdenum Steel

ASTM A752 Grade 8620 Annealed

Nickel Chromium Molybdenum Steel

ASTM A837 Grade 8620

Nickel Chromium Molybdenum Steel

ASTM A506 Grade 8620

Chromium Molybdenum Steel

SAE J404 Grade 8620

Nickel Chromium Molybdenum Steel

ASTM A304 Grade 8617H