Wrought Copper Pure / Low Alloyed Copper
EN 1977 Grade Cu-HCP H040Wrought Copper Pure / Low Alloyed Copper
ASTM B743 Grade C10800 O50Wrought Copper Pure / Low Alloyed Copper
ASTM B743 Grade C10800 O60Wrought Copper Pure / Low Alloyed Copper
ASTM B187 Grade C10800 O60Wrought Copper Pure / Low Alloyed Copper
ASTM B75 Grade C10800 O50Wrought Copper Pure / Low Alloyed Copper
ASTM B75 Grade C10800 O60Wrought Copper Pure / Low Alloyed Copper
ASTM B152 Grade C10800 H04Wrought Copper Pure / Low Alloyed Copper
ASTM B152 Grade C10800 H08Wrought Copper Pure / Low Alloyed Copper
ASTM B152 Grade C10800 M20Wrought Copper Pure / Low Alloyed Copper
ASTM B187 Grade C10800 H04Wrought Copper Pure / Low Alloyed Copper
ASTM B272 Grade C10800 H04Wrought Copper Pure / Low Alloyed Copper
ASTM B272 Grade C10800 O61Wrought Copper Pure / Low Alloyed Copper
ASTM B152 Grade C10800 H00Wrought Copper Pure / Low Alloyed Copper
ASTM B152 Grade C10800 H01Wrought Copper Pure / Low Alloyed Copper
ASTM B152 Grade C10800 H02Wrought Copper Pure / Low Alloyed Copper
ASTM B152 Grade C10800 H03Wrought Copper Pure / Low Alloyed Copper
ASTM B152 Grade C10800 H06Wrought Copper Pure / Low Alloyed Copper
ASTM B152 Grade C10800 H10Wrought Copper Pure / Low Alloyed Copper
ASTM B152 Grade C10800 O25Wrought Copper Pure / Low Alloyed Copper
ASTM B743 Grade C10800 H58