This website uses cookies to improve service quality. You will find more information about cookies on the privacy policy page.
Elongation A50 A50
0 - 25 % at 20 °C
Hardness, Rockwell C HRC
0 - 50 [-] at 20 °C
Tensile strength Rm
195 - 255 MPa at 20 °C
Yield strength YS
0 - 55 MPa at 20 °C
Element
Weight %
Comment
5E-3 - 0.01 %
0 - 99.95 %
This material data has been provided by ASTM.