Nickel Chromium Iron Alloy
Sanicro 31HTSuministrada por:
Alleima (formerly Sandvik Materials Technology)Acero inoxidable austenítico
EN 10028-7 Grade X8NiCrAlTi32-21 solution annealed (+AT)Acero inoxidable austenítico
EN 10028-7 Grade X5NiCrAlTi31-20 recrystallization annealed (+RA)Acero inoxidable austenítico
EN 10028-7 Grade X5NiCrAlTi31-20 solution annealed (+AT)Acero inoxidable austenítico
EN 10095 Grade X10NiCrAlTi32-21 solution annealed (+AT)