Acero inoxidable dúplex
S31803 / COLDUPLEX Duplex Stainless SteelSuperaustenitic Stainless Steel
Sandvik 254 SMOSuministrada por:
Alleima (formerly Sandvik Materials Technology)Acero inoxidable martensítico
ASTM A473 Grade 410S AnnealedAcero inoxidable martensítico
ASTM A473 Grade 416 AnnealedAcero inoxidable ferrítico
ASTM A473 Grade 430 AnnealedAcero inoxidable ferrítico
ASTM A473 Grade 446 AnnealedAcero inoxidable martensítico
ASTM A473 Grade 403 AnnealedAcero inoxidable ferrítico
ASTM A473 Grade 405 AnnealedAcero inoxidable martensítico
ASTM A473 Grade 410 AnnealedAcero inoxidable martensítico
ASTM A473 Grade 416 Se AnnealedAcero inoxidable ferrítico
ASTM A473 Grade 429 AnnealedAcero inoxidable ferrítico
ASTM A473 Grade 430F Se AnnealedAcero inoxidable martensítico
ASTM A473 Grade 430F AnnealedAcero inoxidable martensítico
ASTM A473 Grade S41425 TemperedAcero inoxidable martensítico
ASTM A473 Grade S41500 Normalized and temperedAcero inoxidable austenítico
ASTM A473 Grade S30815 AnnealedAcero inoxidable austenítico
ASTM A473 Grade XM-10 AnnealedAcero inoxidable austenítico
ASTM A473 Grade 309 AnnealedAcero inoxidable austenítico
ASTM A473 Grade 310 Annealed