Unclassified Low Alloy Steel
EN 10225 Grade S420G1 quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Unclassified Low Alloy Steel
EN 10225 Grade S355G7 thermomechanically rolledSuministrada por:
1 proveedor Matmatch
Unclassified Low Alloy Steel
EN 10225 Grade S420G1 thermomechanically rolledSuministrada por:
1 proveedor Matmatch
Unclassified Low Alloy Steel
EN 10225 Grade S460G1 thermomechanically rolledSuministrada por:
1 proveedor Matmatch
Acero bajo en carbono
EN 10225 Grade S355G13 normalized or normalized formed (+N)Acero bajo en carbono
EN 10225 Grade S355G13 quenched and tempered (+QT)Medium Carbon Steel
EN 10225 Grade S355G14 normalized or normalized formed (+N)Medium Carbon Steel
EN 10225 Grade S355G15 normalized or normalized formed (+N)Medium Carbon Steel
EN 10225 Grade S355G14 quenched and tempered (+QT)Medium Carbon Steel
EN 10225 Grade S355G15 quenched and tempered (+QT)Unclassified Low Alloy Steel
EN 10225 Grade S355G7 normalized or normalized formed (+N)Suministrada por:
ArcelorMittalUnclassified Low Alloy Steel
EN 10225 Grade S355G7 thermomechanically rolled (+M)Suministrada por:
ArcelorMittalUnclassified Low Alloy Steel
EN 10225 Grade S355G8 normalized or normalized formed (+N)Suministrada por:
ArcelorMittalUnclassified Low Alloy Steel
EN 10225 Grade S355G8 thermomechanically rolled (+M)Suministrada por:
ArcelorMittalUnclassified Low Alloy Steel
EN S355G10 thermomechanically rolled (+M)Suministrada por:
ArcelorMittalUnclassified Low Alloy Steel
EN 10225 Grade S355G9 normalized or normalized formed (+N)Suministrada por:
ArcelorMittalUnclassified Low Alloy Steel
EN 10225 Grade S355G9 thermomechanically rolled (+M)Suministrada por:
ArcelorMittalUnclassified Low Alloy Steel
EN 10225 Grade S355G10 normalized or normalized formed (+N)Suministrada por:
ArcelorMittalUnclassified Low Alloy Steel
EN 10225 Grade S355G2 normalized or normalized formed (+N)Suministrada por:
ArcelorMittalUnclassified Low Alloy Steel
EN 10225 Grade S355G3 normalized or normalized formed (+N)Suministrada por:
ArcelorMittal