General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 3.45 g/cm³ Show Supplier Material materials with Densidad of 3.45 g/cm³ |
Chemical properties
Property | Value | Comment |
---|---|---|
Boro | 40 - 41.9 % Show Supplier Material materials with Boro of 40 - 41.9 % | |
Calcio | 0.2 - 2 % Show Supplier Material materials with Calcio of 0.2 - 2 % | |
Nitrógeno | 50 - 58.3 % Show Supplier Material materials with Nitrógeno of 50 - 58.3 % | |
Otro | 0.2 - 0.3 % Show Supplier Material materials with Otro of 0.2 - 0.3 % | Chloride, Iron, Aluminum, Silicon |
Oxígeno | 0.3 - 3 % Show Supplier Material materials with Oxígeno of 0.3 - 3 % |