General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 5.68 g/cm³ Show Supplier Material materials with Densidad of 5.68 g/cm³ |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 0.1 - 0.4 % Show Supplier Material materials with Aluminio of 0.1 - 0.4 % | as Alumina |
Circonio | 90 - 95 % Show Supplier Material materials with Circonio of 90 - 95 % | as Zirconia |
Itrio | 4 - 5 % Show Supplier Material materials with Itrio of 4 - 5 % | as Yttria |
Otro | 0.2 % Show Supplier Material materials with Otro of 0.2 % | Titania, Calcium Oxide, Iron Oxide, Sodium Oxide |
Silicona | 0.01 - 0.05 % Show Supplier Material materials with Silicona of 0.01 - 0.05 % | as Silica |