General
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Densidad | 2.7 g/cm³ Show Material materials with Densidad of 2.7 g/cm³ | H18 | EN 573-3, EN 683 | Strip, Sheet |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 6000 Series Aluminium | ||||
Módulo de cizallamiento | 26.0 - 26.5 GPa Show Material materials with Módulo de cizallamiento of 26.0 - 26.5 GPa | Typical for Wrought 6000 Series Aluminium | ||||
Módulo elástico | 70.0 GPa Show Material materials with Módulo elástico of 70.0 GPa | Typical for Wrought 6000 Series Aluminium | ||||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 6000 Series Aluminium | ||||
Resistencia a la tracción | 160.0 MPa Show Material materials with Resistencia a la tracción of 160.0 MPa | H18 | EN 573-3, EN 683 | Strip, Sheet | ||
20.0 °C | 160.0 MPa Show Material materials with Resistencia a la tracción of 160.0 MPa | H18 | EN 573-3 | Foil |
Aplicaciones térmicas
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Calor específico | 887.0 - 963.0 J/(kg·K) Show Material materials with Calor específico of 887.0 - 963.0 J/(kg·K) | Typical for Wrought 6000 Series Aluminium | ||||
Coeficiente de dilatación térmica | 20 °C | 2.3399999999999996e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.3399999999999996e-05 1/K | H18 | EN 573-3, EN 683 | Strip, Sheet | |
100 °C | 2.3399999999999996e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.3399999999999996e-05 1/K | H18 | EN 573-3, EN 683 | Strip, Sheet | ||
Conductividad térmica | 197.0 - 213.0 W/(m·K) Show Material materials with Conductividad térmica of 197.0 - 213.0 W/(m·K) | H18 | EN 573-3, EN 683 | Strip, Sheet | ||
Temperatura de fusión | 615.0 - 655.0 °C Show Material materials with Temperatura de fusión of 615.0 - 655.0 °C | H18 | EN 573-3, EN 683 | Strip, Sheet |
Eléctrico
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Conductividad eléctrica | 30000000.0 - 32000000.0 S/m Show Material materials with Conductividad eléctrica of 30000000.0 - 32000000.0 S/m | H18 | EN 573-3, EN 683 | Strip, Sheet |
Resistividad eléctrica | 3.13e-08 - 3.33e-08 Ω·m Show Material materials with Resistividad eléctrica of 3.13e-08 - 3.33e-08 Ω·m | H18 | EN 573-3, EN 683 | Strip, Sheet |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Cobre | 0.15 - 0.4 % Show Material materials with Cobre of 0.15 - 0.4 % | H18 | EN 573-3, EN 683 | Foil, Strip, Sheet |
Hierro | 0.8 % Show Material materials with Hierro of 0.8 % | H18 | EN 573-3 | Foil |
0.80 % Show Material materials with Hierro of 0.80 % | H18 | EN 573-3, EN 683 | Strip, Sheet | |
Magnesio | 0.4 - 0.8 % Show Material materials with Magnesio of 0.4 - 0.8 % | H18 | EN 573-3, EN 683 | Foil, Strip, Sheet |
Manganeso | 0.1 % Show Material materials with Manganeso of 0.1 % | H18 | EN 573-3, EN 683 | Foil, Strip, Sheet |
Silicona | 0.2 - 0.5 % Show Material materials with Silicona of 0.2 - 0.5 % | H18 | EN 573-3, EN 683 | Foil, Strip, Sheet |
Zinc | 0.2 % Show Material materials with Zinc of 0.2 % | H18 | EN 573-3, EN 683 | Foil, Strip, Sheet |
Technological properties
Property | ||
---|---|---|
Workability | Excellent workability. |