Chemical properties
Property | Value |
---|---|
Circonio | 0.1 - 1 % Show Material materials with Circonio of 0.1 - 1 % |
Cobre | 0.03 % Show Material materials with Cobre of 0.03 % |
Hierro | 0.01 % Show Material materials with Hierro of 0.01 % |
Itrio | 4.75 - 5.5 % Show Material materials with Itrio of 4.75 - 5.5 % |
Litio | 0.2 % Show Material materials with Litio of 0.2 % |
Manganeso | 0.15 % Show Material materials with Manganeso of 0.15 % |
Níquel | 5E-3 % Show Material materials with Níquel of 5E-3 % |
Silicona | 0.01 % Show Material materials with Silicona of 0.01 % |
Tierras raras | 1.5 - 4 % Show Material materials with Tierras raras of 1.5 - 4 % |
Zinc | 0.2 % Show Material materials with Zinc of 0.2 % |