Chemical properties
Property | Value |
---|---|
Aluminio | 2.5 - 3.5 % Show Material materials with Aluminio of 2.5 - 3.5 % |
Cobre | 0.1 % Show Material materials with Cobre of 0.1 % |
Hierro | 0.03 % Show Material materials with Hierro of 0.03 % |
Manganeso | 0.05 - 0.4 % Show Material materials with Manganeso of 0.05 - 0.4 % |
Níquel | 5E-3 % Show Material materials with Níquel of 5E-3 % |
Silicona | 0.1 % Show Material materials with Silicona of 0.1 % |
Zinc | 0.5 - 1.5 % Show Material materials with Zinc of 0.5 - 1.5 % |