General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.74 g/cm³ Show Material materials with Densidad of 1.74 g/cm³ | Typical for Pure Magnesium |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Magnesium |
Módulo de cizallamiento | 23.0 °C | 45 GPa Show Material materials with Módulo de cizallamiento of 45 GPa | Typical for Magnesium |
Módulo elástico | 23.0 °C | 40 - 45 GPa Show Material materials with Módulo elástico of 40 - 45 GPa | Typical for Pure Magnesium |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 1010 - 1050 J/(kg·K) Show Material materials with Calor específico of 1010 - 1050 J/(kg·K) | Typical for Pure Magnesium |
Coeficiente de dilatación térmica | 23.0 °C | 2.5E-5 - 2.6E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 2.5E-5 - 2.6E-5 1/K | Typical for Pure Magnesium |
Conductividad térmica | 23.0 °C | 153 - 167 W/(m·K) Show Material materials with Conductividad térmica of 153 - 167 W/(m·K) | Typical for Pure Magnesium |
Temperatura de fusión | 650 °C Show Material materials with Temperatura de fusión of 650 °C | Typical for Pure Magnesium |
Chemical properties
Property | Value |
---|---|
Aluminio | 4E-3 % Show Material materials with Aluminio of 4E-3 % |
Boro | 3E-5 % Show Material materials with Boro of 3E-5 % |
Cobre | 5E-4 % Show Material materials with Cobre of 5E-4 % |
Hierro | 2E-3 % Show Material materials with Hierro of 2E-3 % |
Magnesio | 99.98 % Show Material materials with Magnesio of 99.98 % |
Manganeso | 2E-3 % Show Material materials with Manganeso of 2E-3 % |
Níquel | 5E-4 % Show Material materials with Níquel of 5E-4 % |
Otro | each 0.005, For applications in nuclear energy technology: cadmium and boron should be limited to: Ca 0.0001 or 0.00005. B 0.00007 or 0.00003 |
Plomo | 1E-3 % Show Material materials with Plomo of 1E-3 % |
Silicona | 3E-3 % Show Material materials with Silicona of 3E-3 % |
Titanio | 1E-3 % Show Material materials with Titanio of 1E-3 % |