General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.74 g/cm³ Show Material materials with Densidad of 1.74 g/cm³ | Typical for Magnesium |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Magnesium |
Módulo de cizallamiento | 23.0 °C | 45 GPa Show Material materials with Módulo de cizallamiento of 45 GPa | Typical for Magnesium |
Módulo elástico | 23.0 °C | 45 GPa Show Material materials with Módulo elástico of 45 GPa | Typical for Magnesium |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 1010 - 1060 J/(kg·K) Show Material materials with Calor específico of 1010 - 1060 J/(kg·K) | Typical for Magnesium |
Coeficiente de dilatación térmica | 23.0 °C | 1.3E-5 - 2.6E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.3E-5 - 2.6E-5 1/K | Typical for Magnesium |
Conductividad térmica | 23.0 °C | 153 - 167 W/(m·K) Show Material materials with Conductividad térmica of 153 - 167 W/(m·K) | Typical for Magnesium |
Temperatura de fusión | 650 °C Show Material materials with Temperatura de fusión of 650 °C | Typical for Magnesium |
Chemical properties
Property | Value |
---|---|
Aluminio | 4.5 - 5.5 % Show Material materials with Aluminio of 4.5 - 5.5 % |
Berilio | 5E-4 - 1.5E-3 % Show Material materials with Berilio of 5E-4 - 1.5E-3 % |
Cobre | 0.01 % Show Material materials with Cobre of 0.01 % |
Hierro | 4E-3 % Show Material materials with Hierro of 4E-3 % |
Manganeso | 0.24 - 0.6 % Show Material materials with Manganeso of 0.24 - 0.6 % |
Níquel | 1E-3 % Show Material materials with Níquel of 1E-3 % |
Otro | each 0.01. Rest Mg, This alloy is a patented alloying composition for elevated temperature applications., if the minimum Mn or maximum Fe content does not meet the specifications, then the Fe/Mg ratio must not exceed 0.021 |
Silicona | 0.08 - 0.1 % Show Material materials with Silicona of 0.08 - 0.1 % |
Zinc | 0.2 - 0.22 % Show Material materials with Zinc of 0.2 - 0.22 % |