General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.7 g/cm³ Show Material materials with Densidad of 1.7 g/cm³ | Typical for Cast Rare Earth Grade |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Magnesium |
Módulo de cizallamiento | 23.0 °C | 45 GPa Show Material materials with Módulo de cizallamiento of 45 GPa | Typical for Magnesium |
Módulo elástico | 23.0 °C | 40 - 45 GPa Show Material materials with Módulo elástico of 40 - 45 GPa | Typical for Cast Rare Earth Grade |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 966 - 1050 J/(kg·K) Show Material materials with Calor específico of 966 - 1050 J/(kg·K) | Typical for Cast Rare Earth Grade |
Coeficiente de dilatación térmica | 23.0 °C | 2.6E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 2.6E-5 1/K | Typical for Cast Rare Earth Grade |
Conductividad térmica | 23.0 °C | 51 - 113 W/(m·K) Show Material materials with Conductividad térmica of 51 - 113 W/(m·K) | Typical for Cast Rare Earth Grade |
Temperatura de fusión | 535 - 645 °C Show Material materials with Temperatura de fusión of 535 - 645 °C | Typical for Cast Rare Earth Grade |
Chemical properties
Property | Value |
---|---|
Circonio | 0.3 - 1 % Show Material materials with Circonio of 0.3 - 1 % |
Cobre | 0.03 % Show Material materials with Cobre of 0.03 % |
Hierro | 0.01 % Show Material materials with Hierro of 0.01 % |
Itrio | 3.7 - 4.3 % Show Material materials with Itrio of 3.7 - 4.3 % |
Litio | 0.18 - 0.2 % Show Material materials with Litio of 0.18 - 0.2 % |
Manganeso | 0.15 % Show Material materials with Manganeso of 0.15 % |
Neodimio | 2 - 2.5 % Show Material materials with Neodimio of 2 - 2.5 % |
Níquel | 5E-3 % Show Material materials with Níquel of 5E-3 % |
Otro | each 0.2. Rest Mg, Other rare earth metals should in principle be heavy rare earths, such as gadolinium, dysprosium, erbium and ytterbium. Other rare earth elements are derived from yttrium, typically 80 % Yttrium and 20 % heavy rare earth metals.,total 0.30. Rest Mg, Other rare earth metals should in principle be heavy rare earths, such as gadolinium, dysprosium, erbium and ytterbium. Other rare earth elements are derived from yttrium, typically 80 % Yttrium and 20 % heavy rare earth metals. |
Silicona | 0.01 % Show Material materials with Silicona of 0.01 % |
Zinc | 0.2 % Show Material materials with Zinc of 0.2 % |