General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 9.8 g/cm³ Show Material materials with Densidad of 9.8 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 23.0 °C | 18 [-] Show Material materials with Dureza Brinell of 18 [-] |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 130 - 159 J/(kg·K) Show Material materials with Calor específico of 130 - 159 J/(kg·K) | Typical for Lead Antimony |
Conductividad térmica | 23.0 °C | 24 - 34 W/(m·K) Show Material materials with Conductividad térmica of 24 - 34 W/(m·K) | Typical for Lead Antimony |
Temperatura de fusión | 235 - 305 °C Show Material materials with Temperatura de fusión of 235 - 305 °C | Typical for Lead Antimony |
Chemical properties
Property | Value |
---|---|
Antimonio | 8 - 11 % Show Material materials with Antimonio of 8 - 11 % |
Arsénico | 0.05 % Show Material materials with Arsénico of 0.05 % |
Bismuto | 0.05 % Show Material materials with Bismuto of 0.05 % |
Cadmio | 1E-3 % Show Material materials with Cadmio of 1E-3 % |
Cobre | 0.05 % Show Material materials with Cobre of 0.05 % |
Estaño | 4 - 6 % Show Material materials with Estaño of 4 - 6 % |
Otro | Other impurities: Total 0.1. individually 0.03. Rest Pb., The age hardening of Pb-Sb alloys can be improved by arsenic, for casting alloys 0.08 to 0.15 % As are recommended. |
Plata | 8E-3 % Show Material materials with Plata of 8E-3 % |