General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 9.4 g/cm³ Show Material materials with Densidad of 9.4 g/cm³ |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 213 - 239 J/(kg·K) Show Material materials with Calor específico of 213 - 239 J/(kg·K) | Typical for Lead Tin |
Conductividad térmica | 23.0 °C | 35 - 57 W/(m·K) Show Material materials with Conductividad térmica of 35 - 57 W/(m·K) | Typical for Lead Tin |
Temperatura de fusión | 186 - 235 °C Show Material materials with Temperatura de fusión of 186 - 235 °C |
Chemical properties
Property | Value |
---|---|
Aluminio | 1E-3 % Show Material materials with Aluminio of 1E-3 % |
Antimonio | 0.5 - 2 % Show Material materials with Antimonio of 0.5 - 2 % |
Arsénico | 0.03 % Show Material materials with Arsénico of 0.03 % |
Bismuto | 0.25 % Show Material materials with Bismuto of 0.25 % |
Cadmio | 1E-3 % Show Material materials with Cadmio of 1E-3 % |
Cobre | 0.08 % Show Material materials with Cobre of 0.08 % |
Estaño | 34.5 - 35.5 % Show Material materials with Estaño of 34.5 - 35.5 % |
Hierro | 0.02 % Show Material materials with Hierro of 0.02 % |
Indio | 0.1 % Show Material materials with Indio of 0.1 % |
Níquel | 0.01 % Show Material materials with Níquel of 0.01 % |
Oro | 0.05 % Show Material materials with Oro of 0.05 % |
Otro | Rest Pb |
Plata | 0.1 % Show Material materials with Plata of 0.1 % |
Zinc | 1E-3 % Show Material materials with Zinc of 1E-3 % |