General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8 g/cm³ Show Material materials with Densidad of 8 g/cm³ |
Mecánica
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Conductividad térmica | 23.0 °C | 40 W/(m·K) Show Material materials with Conductividad térmica of 40 W/(m·K) | Typical for Tin Antimony |
Temperatura de fusión | 215 - 350 °C Show Material materials with Temperatura de fusión of 215 - 350 °C | Typical for Tin Antimony |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.01 % Show Material materials with Aluminio of 0.01 % |
Antimonio | 12 - 14 % Show Material materials with Antimonio of 12 - 14 % |
Arsénico | 0.08 % Show Material materials with Arsénico of 0.08 % |
Cobre | 2 - 3 % Show Material materials with Cobre of 2 - 3 % |
Estaño | 49 - 51 % Show Material materials with Estaño of 49 - 51 % |
Hierro | 0.08 % Show Material materials with Hierro of 0.08 % |
Otro | Rest Pb |
Zinc | 0.01 % Show Material materials with Zinc of 0.01 % |