General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.13 g/cm³ Show Material materials with Densidad of 7.13 g/cm³ | Typical for Zinc |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.25 [-] Show Material materials with Coeficiente de Poisson of 0.25 [-] | Typical for Zinc |
Módulo de cizallamiento | 23.0 °C | 42 GPa Show Material materials with Módulo de cizallamiento of 42 GPa | Typical for Zinc |
Módulo elástico | 23.0 °C | 105 GPa Show Material materials with Módulo elástico of 105 GPa | Typical for Zinc |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 272 - 525 J/(kg·K) Show Material materials with Calor específico of 272 - 525 J/(kg·K) | Typical for Zinc |
Coeficiente de dilatación térmica | 23.0 °C | 2.2E-5 - 2.8E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 2.2E-5 - 2.8E-5 1/K | Typical for Zinc |
Conductividad térmica | 23.0 °C | 105 - 125 W/(m·K) Show Material materials with Conductividad térmica of 105 - 125 W/(m·K) | Typical for Zinc |
Temperatura de fusión | 380 - 420 °C Show Material materials with Temperatura de fusión of 380 - 420 °C | Typical for Zinc |
Chemical properties
Property | Value |
---|---|
Cadmio | 5E-3 % Show Material materials with Cadmio of 5E-3 % |
Hierro | 0.05 % Show Material materials with Hierro of 0.05 % |
Otro | Zn corresponds to the nominal zinc composition, sum of the elements Pb, Cd, Fe, Sn, Cu and Al max. 1.5 |
Plomo | 1.4 % Show Material materials with Plomo of 1.4 % |
Zinc | 98.5 % Show Material materials with Zinc of 98.5 % |