General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 7.1 g/cm³ Show Material materials with Densidad of 7.1 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.25 [-] Show Material materials with Coeficiente de Poisson of 0.25 [-] | Typical for Zinc |
Módulo de cizallamiento | 23.0 °C | 42 GPa Show Material materials with Módulo de cizallamiento of 42 GPa | Typical for Zinc |
Módulo elástico | 23.0 °C | 105 GPa Show Material materials with Módulo elástico of 105 GPa | Typical for Zinc |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 272 - 525 J/(kg·K) Show Material materials with Calor específico of 272 - 525 J/(kg·K) | Typical for Zinc |
Coeficiente de dilatación térmica | 23.0 °C | 2.2E-5 - 2.8E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 2.2E-5 - 2.8E-5 1/K | Typical for Zinc |
Conductividad térmica | 23.0 °C | 105 - 125 W/(m·K) Show Material materials with Conductividad térmica of 105 - 125 W/(m·K) | Typical for Zinc |
Temperatura de fusión | 195 - 385 °C Show Material materials with Temperatura de fusión of 195 - 385 °C |
Chemical properties
Property | Value |
---|---|
Aluminio | 1E-3 % Show Material materials with Aluminio of 1E-3 % |
Antimonio | 0.1 % Show Material materials with Antimonio of 0.1 % |
Arsénico | 0.03 % Show Material materials with Arsénico of 0.03 % |
Bismuto | 0.1 % Show Material materials with Bismuto of 0.1 % |
Cadmio | 1E-3 % Show Material materials with Cadmio of 1E-3 % |
Cobre | 0.1 % Show Material materials with Cobre of 0.1 % |
Estaño | 19 - 21 % Show Material materials with Estaño of 19 - 21 % |
Hierro | 0.02 % Show Material materials with Hierro of 0.02 % |
Indio | 0.1 % Show Material materials with Indio of 0.1 % |
Níquel | 0.01 % Show Material materials with Níquel of 0.01 % |
Oro | 0.05 % Show Material materials with Oro of 0.05 % |
Otro | Rest Zn |
Plata | 0.1 % Show Material materials with Plata of 0.1 % |
Plomo | 0.1 % Show Material materials with Plomo of 0.1 % |