Aplicaciones térmicas
Property | Value |
---|---|
Temperatura de fusión | 980 - 1060 °C Show Material materials with Temperatura de fusión of 980 - 1060 °C |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.05 % Show Material materials with Aluminio of 0.05 % |
Azufre | 0.02 % Show Material materials with Azufre of 0.02 % |
Boro | 2.75 - 3.5 % Show Material materials with Boro of 2.75 - 3.5 % |
Cadmio | 0.01 % Show Material materials with Cadmio of 0.01 % |
Carbono | 0.6 - 0.9 % Show Material materials with Carbono of 0.6 - 0.9 % |
Circonio | 0.05 % Show Material materials with Circonio of 0.05 % |
Cobalto | 0.1 % Show Material materials with Cobalto of 0.1 % |
Cromo | 13 - 15 % Show Material materials with Cromo of 13 - 15 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Hierro | 4 - 5 % Show Material materials with Hierro of 4 - 5 % |
Otro | Andere Beimengungen: zusammen 0,50, Rest Ni |
Plomo | 0.03 % Show Material materials with Plomo of 0.03 % |
Selenio | 5E-3 % Show Material materials with Selenio of 5E-3 % |
Silicona | 4 - 5 % Show Material materials with Silicona of 4 - 5 % |
Titanio | 0.05 % Show Material materials with Titanio of 0.05 % |