General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 9.2 g/cm³ Show Material materials with Densidad of 9.2 g/cm³ | Typical for Nickel Molybdenum Alloy |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Módulo elástico | 23.0 °C | 220 GPa Show Material materials with Módulo elástico of 220 GPa | Typical for Nickel Molybdenum Alloy |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 377 - 439 J/(kg·K) Show Material materials with Calor específico of 377 - 439 J/(kg·K) | Typical for Nickel Molybdenum Alloy |
Coeficiente de dilatación térmica | 23.0 °C | 7.6E-6 - 1.7E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 7.6E-6 - 1.7E-5 1/K | Typical for Nickel Molybdenum Alloy |
Conductividad térmica | 23.0 °C | 9 - 15 W/(m·K) Show Material materials with Conductividad térmica of 9 - 15 W/(m·K) | Typical for Nickel Molybdenum Alloy |
Temperatura de fusión | 1560 °C Show Material materials with Temperatura de fusión of 1560 °C | Typical for Nickel Molybdenum Alloy |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.1 - 0.5 % Show Material materials with Aluminio of 0.1 - 0.5 % |
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Carbono | 0.01 % Show Material materials with Carbono of 0.01 % |
Cobalto | 3 % Show Material materials with Cobalto of 3 % |
Cobre | 0.5 % Show Material materials with Cobre of 0.5 % |
Cromo | 0.5 - 3 % Show Material materials with Cromo of 0.5 - 3 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Hierro | 1 - 6 % Show Material materials with Hierro of 1 - 6 % |
Manganeso | 3 % Show Material materials with Manganeso of 3 % |
Molibdeno | 26 - 32 % Show Material materials with Molibdeno of 26 - 32 % |
Níquel | 65 % Show Material materials with Níquel of 65 % |
Otro | Nb + Ta 0.40 |
Silicona | 0.1 % Show Material materials with Silicona of 0.1 % |
Titanio | 0.2 % Show Material materials with Titanio of 0.2 % |
Vanadio | 0.2 % Show Material materials with Vanadio of 0.2 % |
Wolframio | 3 % Show Material materials with Wolframio of 3 % |