General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.75 - 8.4 g/cm³ Show Material materials with Densidad of 7.75 - 8.4 g/cm³ | Typical for Nickel Chromium Iron Alloy |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Módulo elástico | 23.0 °C | 150 GPa Show Material materials with Módulo elástico of 150 GPa | Typical for Nickel Chromium Iron Alloy |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 285 - 545 J/(kg·K) Show Material materials with Calor específico of 285 - 545 J/(kg·K) | Typical for Nickel Chromium Iron Alloy |
Coeficiente de dilatación térmica | 23.0 °C | 7.6E-6 - 1.7E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 7.6E-6 - 1.7E-5 1/K | Typical for Nickel Chromium Iron Alloy |
Conductividad térmica | 23.0 °C | 8 - 35 W/(m·K) Show Material materials with Conductividad térmica of 8 - 35 W/(m·K) | Typical for Nickel Chromium Iron Alloy |
Temperatura de fusión | 1200 - 1480 °C Show Material materials with Temperatura de fusión of 1200 - 1480 °C | Typical for Nickel Chromium Iron Alloy |
Chemical properties
Property | Value |
---|---|
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Carbono | 0.03 - 0.08 % Show Material materials with Carbono of 0.03 - 0.08 % |
Cobalto | 2.5 - 4 % Show Material materials with Cobalto of 2.5 - 4 % |
Cromo | 24 - 26 % Show Material materials with Cromo of 24 - 26 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 2 % Show Material materials with Manganeso of 2 % |
Molibdeno | 2.5 - 4 % Show Material materials with Molibdeno of 2.5 - 4 % |
Níquel | 44 - 47 % Show Material materials with Níquel of 44 - 47 % |
Otro | Rest Fe |
Silicona | 0.7 - 1.5 % Show Material materials with Silicona of 0.7 - 1.5 % |
Wolframio | 2.5 - 4 % Show Material materials with Wolframio of 2.5 - 4 % |