General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 8.7 g/cm³ Show Material materials with Densidad of 8.7 g/cm³ | Typical for Nickel Chromium Molybdenum Alloy |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Módulo elástico | 23.0 °C | 207 GPa Show Material materials with Módulo elástico of 207 GPa | Typical for Nickel Chromium Molybdenum Alloy |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 285 - 545 J/(kg·K) Show Material materials with Calor específico of 285 - 545 J/(kg·K) | Typical for Nickel Chromium Molybdenum Alloy |
Coeficiente de dilatación térmica | 23.0 °C | 7.6E-6 - 1.7E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 7.6E-6 - 1.7E-5 1/K | Typical for Nickel Chromium Molybdenum Alloy |
Conductividad térmica | 23.0 °C | 8 - 35 W/(m·K) Show Material materials with Conductividad térmica of 8 - 35 W/(m·K) | Typical for Nickel Chromium Molybdenum Alloy |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.2 - 0.5 % Show Material materials with Aluminio of 0.2 - 0.5 % |
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Boro | 0.015 % Show Material materials with Boro of 0.015 % |
Carbono | 0.05 - 0.15 % Show Material materials with Carbono of 0.05 - 0.15 % |
Cobalto | 5 % Show Material materials with Cobalto of 5 % |
Cobre | 0.5 % Show Material materials with Cobre of 0.5 % |
Cromo | 20 - 24 % Show Material materials with Cromo of 20 - 24 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Hierro | 3 % Show Material materials with Hierro of 3 % |
Manganeso | 0.3 - 1 % Show Material materials with Manganeso of 0.3 - 1 % |
Molibdeno | 1 - 3 % Show Material materials with Molibdeno of 1 - 3 % |
Otro | Rest Ni, La 0.005 - 0.050 |
Silicona | 0.25 - 0.75 % Show Material materials with Silicona of 0.25 - 0.75 % |
Titanio | 0.1 % Show Material materials with Titanio of 0.1 % |
Wolframio | 13 - 15 % Show Material materials with Wolframio of 13 - 15 % |