General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 8.7 g/cm³ Show Material materials with Densidad of 8.7 g/cm³ | Typical for Nickel Chromium Molybdenum Alloy |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Módulo elástico | 23.0 °C | 207 GPa Show Material materials with Módulo elástico of 207 GPa | Typical for Nickel Chromium Molybdenum Alloy |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 285 - 545 J/(kg·K) Show Material materials with Calor específico of 285 - 545 J/(kg·K) | Typical for Nickel Chromium Molybdenum Alloy |
Coeficiente de dilatación térmica | 23.0 °C | 7.6E-6 - 1.7E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 7.6E-6 - 1.7E-5 1/K | Typical for Nickel Chromium Molybdenum Alloy |
Conductividad térmica | 23.0 °C | 8 - 35 W/(m·K) Show Material materials with Conductividad térmica of 8 - 35 W/(m·K) | Typical for Nickel Chromium Molybdenum Alloy |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.4 % Show Material materials with Aluminio of 0.4 % |
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Carbono | 0.1 % Show Material materials with Carbono of 0.1 % |
Cobalto | 1 % Show Material materials with Cobalto of 1 % |
Cobre | 0.5 % Show Material materials with Cobre of 0.5 % |
Cromo | 20 - 23 % Show Material materials with Cromo of 20 - 23 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Hierro | 5 % Show Material materials with Hierro of 5 % |
Manganeso | 0.5 % Show Material materials with Manganeso of 0.5 % |
Molibdeno | 8 - 10 % Show Material materials with Molibdeno of 8 - 10 % |
Níquel | 58 % Show Material materials with Níquel of 58 % |
Otro | Nb + Ta 3.15 - 4.15. When used according to DIN EN 10095, C must be at least 0.03. |
Silicona | 0.5 % Show Material materials with Silicona of 0.5 % |
Titanio | 0.4 % Show Material materials with Titanio of 0.4 % |