General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.75 - 8.4 g/cm³ Show Material materials with Densidad of 7.75 - 8.4 g/cm³ | Typical for Nickel Chromium Iron Alloy |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Módulo elástico | 23.0 °C | 150 GPa Show Material materials with Módulo elástico of 150 GPa | Typical for Nickel Chromium Iron Alloy |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 285 - 545 J/(kg·K) Show Material materials with Calor específico of 285 - 545 J/(kg·K) | Typical for Nickel Chromium Iron Alloy |
Coeficiente de dilatación térmica | 23.0 °C | 7.6E-6 - 1.7E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 7.6E-6 - 1.7E-5 1/K | Typical for Nickel Chromium Iron Alloy |
Conductividad térmica | 23.0 °C | 8 - 35 W/(m·K) Show Material materials with Conductividad térmica of 8 - 35 W/(m·K) | Typical for Nickel Chromium Iron Alloy |
Temperatura de fusión | 1200 - 1480 °C Show Material materials with Temperatura de fusión of 1200 - 1480 °C | Typical for Nickel Chromium Iron Alloy |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.2 % Show Material materials with Aluminio of 0.2 % |
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Carbono | 0.025 % Show Material materials with Carbono of 0.025 % |
Cobalto | 1 % Show Material materials with Cobalto of 1 % |
Cobre | 1.5 - 3 % Show Material materials with Cobre of 1.5 - 3 % |
Cromo | 19.5 - 23.5 % Show Material materials with Cromo of 19.5 - 23.5 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Manganeso | 1 % Show Material materials with Manganeso of 1 % |
Molibdeno | 2.5 - 3.5 % Show Material materials with Molibdeno of 2.5 - 3.5 % |
Níquel | 38 - 46 % Show Material materials with Níquel of 38 - 46 % |
Otro | Rest Fe |
Silicona | 0.5 % Show Material materials with Silicona of 0.5 % |
Titanio | 0.6 - 1.2 % Show Material materials with Titanio of 0.6 - 1.2 % |