General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 8.1 - 8.2 g/cm³ Show Material materials with Densidad of 8.1 - 8.2 g/cm³ | Typical for Nickel Iron Alloy |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.28 [-] Show Material materials with Coeficiente de Poisson of 0.28 [-] | Typical for Nickel Iron Alloy |
Módulo elástico | 23.0 °C | 137 - 145 GPa Show Material materials with Módulo elástico of 137 - 145 GPa | Typical for Nickel Iron Alloy |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 285 - 545 J/(kg·K) Show Material materials with Calor específico of 285 - 545 J/(kg·K) | Typical for Nickel Iron Alloy |
Coeficiente de dilatación térmica | 23.0 °C | 7.6E-6 - 1.7E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 7.6E-6 - 1.7E-5 1/K | Typical for Nickel Iron Alloy |
Conductividad térmica | 23.0 °C | 8 - 35 W/(m·K) Show Material materials with Conductividad térmica of 8 - 35 W/(m·K) | Typical for Nickel Iron Alloy |
Temperatura de fusión | 1450 °C Show Material materials with Temperatura de fusión of 1450 °C | Typical for Nickel Iron Alloy |
Chemical properties
Property | Value |
---|---|
Carbono | 0.02 % Show Material materials with Carbono of 0.02 % |
Hierro | 44 - 46 % Show Material materials with Hierro of 44 - 46 % |
Manganeso | 0.6 % Show Material materials with Manganeso of 0.6 % |
Otro | Rest Ni, For powder metallurgical production, manganese- and silicon-free materials are also possible. |
Silicona | 0.3 % Show Material materials with Silicona of 0.3 % |