General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 8.9 g/cm³ Show Material materials with Densidad of 8.9 g/cm³ | Typical for Pure/Low Nickel Alloy |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Módulo elástico | 23.0 °C | 190 - 220 GPa Show Material materials with Módulo elástico of 190 - 220 GPa | Typical for Pure/Low Nickel Alloy |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 430 - 532 J/(kg·K) Show Material materials with Calor específico of 430 - 532 J/(kg·K) | Typical for Pure/Low Nickel Alloy |
Coeficiente de dilatación térmica | 23.0 °C | 8.5E-6 - 1.4E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 8.5E-6 - 1.4E-5 1/K | Typical for Pure/Low Nickel Alloy |
Conductividad térmica | 23.0 °C | 18 - 86 W/(m·K) Show Material materials with Conductividad térmica of 18 - 86 W/(m·K) | Typical for Pure/Low Nickel Alloy |
Temperatura de fusión | 1400 - 1500 °C Show Material materials with Temperatura de fusión of 1400 - 1500 °C | Typical for Pure/Low Nickel Alloy |
Chemical properties
Property | Value |
---|---|
Antimonio | 1E-4 % Show Material materials with Antimonio of 1E-4 % |
Arsénico | 1E-3 % Show Material materials with Arsénico of 1E-3 % |
Azufre | 1.5E-3 % Show Material materials with Azufre of 1.5E-3 % |
Bismuto | 1E-4 % Show Material materials with Bismuto of 1E-4 % |
Carbono | 0.015 % Show Material materials with Carbono of 0.015 % |
Cobalto | 0.01 % Show Material materials with Cobalto of 0.01 % |
Cobre | 5E-3 % Show Material materials with Cobre of 5E-3 % |
Estaño | 1E-4 % Show Material materials with Estaño of 1E-4 % |
Fósforo | 1E-3 % Show Material materials with Fósforo of 1E-3 % |
Hierro | 0.02 % Show Material materials with Hierro of 0.02 % |
Manganeso | 5E-4 % Show Material materials with Manganeso of 5E-4 % |
Níquel | 99.96 % Show Material materials with Níquel of 99.96 % |
Otro | The nickel composition includes Co |
Plata | 5E-4 % Show Material materials with Plata of 5E-4 % |
Plomo | 5E-4 % Show Material materials with Plomo of 5E-4 % |
Selenio | 2E-4 % Show Material materials with Selenio of 2E-4 % |
Talio | 1E-4 % Show Material materials with Talio of 1E-4 % |
Telurio | 1E-4 % Show Material materials with Telurio of 1E-4 % |
Tántalo | 5E-4 % Show Material materials with Tántalo of 5E-4 % |
Zinc | 1E-3 % Show Material materials with Zinc of 1E-3 % |