Chemical properties
Property | Value |
---|---|
Antimonio | 1E-3 % Show Material materials with Antimonio of 1E-3 % |
Arsénico | 1E-3 % Show Material materials with Arsénico of 1E-3 % |
Azufre | 2.5E-3 % Show Material materials with Azufre of 2.5E-3 % |
Bismuto | 5E-4 % Show Material materials with Bismuto of 5E-4 % |
Carbono | 0.015 % Show Material materials with Carbono of 0.015 % |
Cobalto | 0.1 % Show Material materials with Cobalto of 0.1 % |
Cobre | 5E-3 % Show Material materials with Cobre of 5E-3 % |
Estaño | 5E-4 % Show Material materials with Estaño of 5E-4 % |
Fósforo | 2E-3 % Show Material materials with Fósforo of 2E-3 % |
Hierro | 0.02 % Show Material materials with Hierro of 0.02 % |
Níquel | 99.95 % Show Material materials with Níquel of 99.95 % |
Otro | The nickel composition includes Co |
Plata | 5E-4 % Show Material materials with Plata of 5E-4 % |
Plomo | 1E-3 % Show Material materials with Plomo of 1E-3 % |
Selenio | 1E-3 % Show Material materials with Selenio of 1E-3 % |
Talio | 5E-4 % Show Material materials with Talio of 5E-4 % |
Telurio | 5E-4 % Show Material materials with Telurio of 5E-4 % |
Zinc | 2E-3 % Show Material materials with Zinc of 2E-3 % |