Chemical properties
Property | Value |
---|---|
Antimonio | 2E-3 % Show Material materials with Antimonio of 2E-3 % |
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % |
Bismuto | 2E-3 % Show Material materials with Bismuto of 2E-3 % |
Carbono | 0.03 % Show Material materials with Carbono of 0.03 % |
Cobalto | 0.5 % Show Material materials with Cobalto of 0.5 % |
Cobre | 0.03 % Show Material materials with Cobre of 0.03 % |
Hierro | 0.03 % Show Material materials with Hierro of 0.03 % |
Níquel | 99.9 % Show Material materials with Níquel of 99.9 % |
Otro | The nickel composition includes Co |
Plomo | 5E-3 % Show Material materials with Plomo of 5E-3 % |