General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 8.9 g/cm³ Show Material materials with Densidad of 8.9 g/cm³ | Typical for Pure/Low Nickel Alloy |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Módulo elástico | 23.0 °C | 190 - 220 GPa Show Material materials with Módulo elástico of 190 - 220 GPa | Typical for Pure/Low Nickel Alloy |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 430 - 532 J/(kg·K) Show Material materials with Calor específico of 430 - 532 J/(kg·K) | Typical for Pure/Low Nickel Alloy |
Coeficiente de dilatación térmica | 23.0 °C | 8.5E-6 - 1.4E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 8.5E-6 - 1.4E-5 1/K | Typical for Pure/Low Nickel Alloy |
Conductividad térmica | 23.0 °C | 18 - 86 W/(m·K) Show Material materials with Conductividad térmica of 18 - 86 W/(m·K) | Typical for Pure/Low Nickel Alloy |
Temperatura de fusión | 1400 - 1500 °C Show Material materials with Temperatura de fusión of 1400 - 1500 °C | Typical for Pure/Low Nickel Alloy |
Chemical properties
Property | Value |
---|---|
Carbono | 1 % Show Material materials with Carbono of 1 % |
Cobre | 1.2 % Show Material materials with Cobre of 1.2 % |
Hierro | 1 % Show Material materials with Hierro of 1 % |
Manganeso | 1.5 % Show Material materials with Manganeso of 1.5 % |
Níquel | 90 % Show Material materials with Níquel of 90 % |
Otro | total 0.2. of which S 0.01. The nickel content includes max. 1.0% Co |
Silicona | 5.5 - 6.5 % Show Material materials with Silicona of 5.5 - 6.5 % |