General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 8.91 - 8.94 g/cm³ Show Material materials with Densidad of 8.91 - 8.94 g/cm³ | Typical for Nickel Copper Alloy |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Módulo elástico | 23.0 °C | 120 - 156 GPa Show Material materials with Módulo elástico of 120 - 156 GPa | Typical for Nickel Copper Alloy |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 418 - 540 J/(kg·K) Show Material materials with Calor específico of 418 - 540 J/(kg·K) | Typical for Nickel Copper Alloy |
Coeficiente de dilatación térmica | 23.0 °C | 1.1E-5 - 1.6E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.1E-5 - 1.6E-5 1/K | Typical for Nickel Copper Alloy |
Conductividad térmica | 23.0 °C | 16 - 45 W/(m·K) Show Material materials with Conductividad térmica of 16 - 45 W/(m·K) | Typical for Nickel Copper Alloy |
Temperatura de fusión | 1170 - 1365 °C Show Material materials with Temperatura de fusión of 1170 - 1365 °C | Typical for Nickel Copper Alloy |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.5 % Show Material materials with Aluminio of 0.5 % |
Azufre | 0.01 % Show Material materials with Azufre of 0.01 % |
Carbono | 0.15 % Show Material materials with Carbono of 0.15 % |
Cobre | 26 - 33 % Show Material materials with Cobre of 26 - 33 % |
Hierro | 1 - 2.5 % Show Material materials with Hierro of 1 - 2.5 % |
Magnesio | 0.12 % Show Material materials with Magnesio of 0.12 % |
Manganeso | 0.5 - 1.5 % Show Material materials with Manganeso of 0.5 - 1.5 % |
Niobio | 1 - 1.5 % Show Material materials with Niobio of 1 - 1.5 % |
Níquel | 62 - 68 % Show Material materials with Níquel of 62 - 68 % |
Otro | total 0.010. The nickel content includes max. 1.0% Co. By adding Nb the cast material becomes weldable |
Plomo | 0.01 % Show Material materials with Plomo of 0.01 % |
Silicona | 0.5 - 1.5 % Show Material materials with Silicona of 0.5 - 1.5 % |
Titanio | 0.2 % Show Material materials with Titanio of 0.2 % |