Chemical properties
Property | Value |
---|---|
Aluminio | 1.5 % Show Material materials with Aluminio of 1.5 % |
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Carbono | 0.15 % Show Material materials with Carbono of 0.15 % |
Cobre | 0.25 % Show Material materials with Cobre of 0.25 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Hierro | 1 % Show Material materials with Hierro of 1 % |
Manganeso | 1 % Show Material materials with Manganeso of 1 % |
Níquel | 92 % Show Material materials with Níquel of 92 % |
Otro | total 0.5., Up to 1 % (mass fraction) of the nickel composition can be present as cobalt., Up to 20 % (mass fraction) of the niobium composition can be replaced by tantalum. |
Silicona | 0.7 % Show Material materials with Silicona of 0.7 % |
Titanio | 2 - 3.5 % Show Material materials with Titanio of 2 - 3.5 % |