Chemical properties
Property | Value |
---|---|
Aluminio | 0.75 - 1.2 % Show Material materials with Aluminio of 0.75 - 1.2 % |
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Boro | 3E-3 % Show Material materials with Boro of 3E-3 % |
Carbono | 0.03 % Show Material materials with Carbono of 0.03 % |
Circonio | 0.02 % Show Material materials with Circonio of 0.02 % |
Cobalto | 1 % Show Material materials with Cobalto of 1 % |
Cobre | 0.3 % Show Material materials with Cobre of 0.3 % |
Cromo | 36 - 39 % Show Material materials with Cromo of 36 - 39 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Hierro | 1 % Show Material materials with Hierro of 1 % |
Manganeso | 0.5 % Show Material materials with Manganeso of 0.5 % |
Molibdeno | 0.5 % Show Material materials with Molibdeno of 0.5 % |
Niobio | 0.25 - 1 % Show Material materials with Niobio of 0.25 - 1 % |
Níquel | 63 % Show Material materials with Níquel of 63 % |
Otro | total 0.5., Up to 1 % (mass fraction) of the nickel composition can be present as cobalt., Up to 20 % (mass fraction) of the niobium composition can be replaced by tantalum. |
Silicona | 0.3 % Show Material materials with Silicona of 0.3 % |
Titanio | 0.25 - 0.75 % Show Material materials with Titanio of 0.25 - 0.75 % |