Chemical properties
Property | Value |
---|---|
Aluminio | 0.4 % Show Material materials with Aluminio of 0.4 % |
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Carbono | 0.08 - 0.15 % Show Material materials with Carbono of 0.08 - 0.15 % |
Cobre | 0.5 % Show Material materials with Cobre of 0.5 % |
Cromo | 19 - 21 % Show Material materials with Cromo of 19 - 21 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Hierro | 2 % Show Material materials with Hierro of 2 % |
Manganeso | 1 % Show Material materials with Manganeso of 1 % |
Níquel | 75 % Show Material materials with Níquel of 75 % |
Otro | total 0.5., Up to 1 % (mass fraction) of the nickel composition can be present as cobalt. |
Silicona | 0.3 % Show Material materials with Silicona of 0.3 % |
Titanio | 0.15 - 0.5 % Show Material materials with Titanio of 0.15 - 0.5 % |