Chemical properties
Property | Value |
---|---|
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Carbono | 0.1 % Show Material materials with Carbono of 0.1 % |
Cobre | 0.5 % Show Material materials with Cobre of 0.5 % |
Cromo | 18 - 22 % Show Material materials with Cromo of 18 - 22 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Hierro | 3 % Show Material materials with Hierro of 3 % |
Manganeso | 2.5 - 3.5 % Show Material materials with Manganeso of 2.5 - 3.5 % |
Niobio | 2 - 3 % Show Material materials with Niobio of 2 - 3 % |
Níquel | 67 % Show Material materials with Níquel of 67 % |
Otro | total 0.5., Up to 1 % (mass fraction) of the nickel composition can be present as cobalt., Up to 20 % (mass fraction) of the niobium composition can be replaced by tantalum. |
Silicona | 0.5 % Show Material materials with Silicona of 0.5 % |
Titanio | 0.7 % Show Material materials with Titanio of 0.7 % |